Piercing is the step in which the plasma arc passes completely through the plate for the first time, before the cut line can begin. In most shops the discussion about cutting parameters centers on current and speed, and piercing stays in the background. Yet this is the stage where consumables carry their highest load, where the first defects on the cut edge form and where thick plate most often costs time. In this article, drawing on our fabrication practice in Lüleburgaz, we look at how plasma cutting piercing works, what risks it carries on thick plate and which methods protect part quality.

What Happens During the Pierce?

Before the cut starts, the torch is positioned at a set height above the plate surface, the arc is ignited and the plasma jet begins to melt the material. Until the plate is fully penetrated, most of the molten metal is not blown along the cut direction but upward, back toward the torch. For this reason the torch tip, nozzle and shield are exposed to far more spatter and heat during the pierce than during normal cutting. Once the pierce is complete, the torch drops to cutting height and the table begins to move.

By its nature, piercing is the most demanding step of plasma cutting. Even at the same current level, travelling along the cut line wears the consumables less than standing in one spot and piercing the plate. In many shops, shortened consumable life is caused not by long cut lines but by a large number of pierces.

Pierce Height and Pierce Delay

During the pierce the torch is held higher than the cutting height, so that molten spatter does not reach the nozzle and shield directly. If the pierce height is too low, spatter sticks to the consumables, the nozzle orifice deteriorates and edge quality drops on later cuts. If it is too high, the arc becomes unstable, the jet disperses and the plate is pierced late or incompletely.

The pierce delay is the time allowed for the arc to penetrate the plate fully, and it grows with thickness. If the delay is too short, the jet has not yet penetrated completely when the table starts moving, and an incomplete cut appears at the start of the line. If it is too long, unnecessary heat builds up at the same point, the melt crater around the hole grows and the consumables wear for no benefit.

These values vary with the machine, power source, gas type and nozzle model. The correct starting point is the cutting chart published by the machine and consumable manufacturer, with fine adjustment in the shop made through test cuts. The balance of current, speed and thickness is a separate subject and is covered in detail in our article on plasma cutting amperage, speed and plate thickness; pierce settings are built on top of that balance.

Risks Specific to Thick Plate

As thickness approaches the upper limit of the selected current class, piercing becomes harder. The jet takes longer to penetrate, more molten metal is blown upward and the consumables wear faster. Three typical problems follow: damage to the nozzle orifice, a wide melt crater around the pierce point and a drop in edge quality at the start of the cut line.

If the plate surface carries rust, oil or weld spatter, arc starting becomes unstable and the same parameters give different results. On warped or wavy plate it is also harder to hold the pierce height constant. Even when the height control system works by sensing the plate surface, a sensing error on thick, bent plate can damage the consumables during the pierce. Checking plate flatness and cleaning the surface before cutting therefore matter for the pierce as well.

Where to Pierce: Using a Lead-in

The pierce point should not be placed on the contour of the finished part. The melt crater and spatter left by the pierce create an irregular zone on the part edge. For this reason, in the cutting program the pierce point is placed a set distance inside the contour or in the scrap area, and the torch starts the cut from there with a lead-in that approaches the contour. For the inner holes of a part the pierce point sits in the scrap of the hole; for the outer contour it sits in the area of the plate outside the part.

The shape of the lead-in also matters. Using a gentle arc or a short tangent entry instead of a sharp one reduces the risk of a notch where the line joins the contour. The lead-out is planned so that it leaves no mark on the contour at the end of the cut. These details directly affect grinding time after cutting.

Edge Starts and Reducing the Number of Pierces

On thick plate, the way to eliminate the pierce altogether is to start the cut from the plate edge whenever possible. In a cut that starts from the edge, the jet does not have to penetrate the plate; no spatter is produced and the load on the consumables drops noticeably. It is not always possible to cut every part this way, but positioning parts near the plate edges during nesting and letting several parts share a common cut line reduces the number of pierces.

Parts with many small holes carry a high total number of pierces. In such jobs, the cutting sequence and the placement and grouping of pierce points affect production time. When consumable life is considered together with the pierce count, it becomes an important component of cost per part.

Monitoring the Consumables

The parts that wear most during piercing are the electrode and the nozzle. Pitting in the electrode, or an enlarged or oval nozzle orifice, disturbs the focus of the jet and lowers both pierce and cut quality. Replacing consumables when cut quality begins to drop, rather than only when they have failed completely, reduces scrap and rework cost. Recording the number of cuts, the number of pierces and the thickness for each set of consumables in the shop makes it easier to predict the replacement time in advance.

Effect on Edge Quality and Downstream Processes

When the pierce is not managed well, problems appear at the start of the cut line: an incomplete cut at the entry, a melt mark around the hole, a notch on the contour and an irregular edge. These defects increase the need for grinding, especially in welded fabrication. The importance of edge quality and heat effect in weld edge preparation is explained in weld edge preparation: oxy-fuel and plasma cutting comparison; choosing the pierce point correctly helps keep the edge that will go to welding clean.

When piercing becomes difficult on very thick plate, the thickness and tolerance of the project may bring oxy-fuel cutting or another method into consideration instead of plasma. Method selection should be made by weighing plate thickness, material type and edge requirement together.

DMK Makina's Approach to the Pierce

Based in Lüleburgaz, DMK Makina serves customers in Thrace and Marmara as well as industrial projects across Turkey and Europe. In CNC plasma cutting, pierce parameters are verified by test cuts according to material type and thickness. In the cutting program, pierce points are moved outside the part contour, edge starts are preferred where suitable and consumables are inspected regularly. DMK Makina is a manufacturing service provider, not a machine seller; parameters are defined in the workshop according to the needs of each job.

Conclusion

Plasma cutting piercing directly affects cut quality and consumable cost, yet it is often overlooked. The correct pierce height and delay, moving the pierce point outside the part contour, starting from the plate edge whenever possible and monitoring consumables regularly improve both edge quality and production time. To get support on the suitable plasma cutting method and parameters for your project, you can contact DMK Makina.